Toolvito

Works on this device

Creep Strain Calculator

At a high temperature a loaded metal keeps stretching slowly with time: this is creep. Work out the steady creep rate from the constants of a power law, the creep strain after a time, the time until a strain limit, and the Larson-Miller parameter that trades temperature against time to rupture.

Enter your values

The steady (secondary) creep rate of a metal under a stress at a high temperature, from the constants of its creep law; and the strain after a time.

Your values

In the units chosen below. From creep tests of your material, a data sheet or a handbook, for this temperature range. No value is built in; the example is for trying the tool.

Often between about 3 and 8 for metals in power-law creep. From creep tests of your material, a data sheet or a handbook, for this temperature range. No value is built in; the example is for trying the tool.

From creep tests of your material, a data sheet or a handbook, for this temperature range. No value is built in; the example is for trying the tool.

With it, the page gives the creep strain after this time at the steady rate.

Your values are worked out in this browser. They are not sent to a server.

Your result will show here

Fill in the values, then choose Calculate.

How to use this calculator

  1. Choose the creep rate from a power law, the strain after a time at a known rate, or the Larson-Miller parameter.
  2. Type the constants of your material (A, n and Q, or C) from creep test data, a data sheet or a handbook, with their units. No material values are built in; Try an example fills example values.
  3. Type the stress, the temperature and the time, and choose Calculate.

The formulas

  • Steady creep rate (power law, Norton, with an Arrhenius term): ε̇ = A × σ^n × exp(−Q ÷ (R T)), with T in kelvin and R = 8.31446 J/(mol·K).
  • Creep strain after a time: ε = ε0 + ε̇ × t, with ε0 the strain at the start of steady creep. Time to a strain limit: t = (εL − ε0) ÷ ε̇.
  • Larson-Miller parameter: LMP = T × (C + log10 t), with T in kelvin (or degrees Rankine) and t in hours. So t = 10^(LMP ÷ T − C) and T = LMP ÷ (C + log10 t).

Worked example

With A = 0.06 per second (σ in MPa), n = 5 and Q = 280 kJ/mol, at 550 °C (823.15 K) and 100 MPa: exp(−Q ÷ RT) = 1.708 × 10⁻¹⁸ and ε̇ = 0.06 × 100⁵ × 1.708 × 10⁻¹⁸ = 1.025 × 10⁻⁹ per second, which is 0.369% per 1,000 hours. After 10,000 hours the creep strain is about 3.69%.

At 550 °C and a rupture time of 100,000 hours with C = 20: LMP = 823.15 × (20 + 5) = 20,579. A material whose master curve gives LMP = 20,000 at your stress lasts 10^(20,000 ÷ 823.15 − 20) = 19,811 hours at 550 °C, or 100,000 hours at 526.85 °C.

All constants here are examples for trying the tool, not the values of a real material.

Limits you should know

  • Creep constants hold only for the stress and temperature range of the tests they were fitted to. Small changes of n and Q change the rate a lot.
  • The strain uses the steady (secondary) rate. The first stage creeps faster at the start, and the last stage speeds up before rupture; neither is modelled here.
  • The Larson-Miller constant C must be the one used for the master curve you read. Long extrapolations beyond the test times are uncertain.
  • For elastic stresses and strains, use the Stress & Strain Calculator; for stresses from held thermal expansion, the Thermal Stress Calculator; for a static check, the Factor of Safety Calculator.
  • This is ideal arithmetic for study and checking, not a design approval and not professional advice.

Related tools