Works on this device
Material Hardness Converter
Hardness scales such as Rockwell, Brinell and Vickers cannot be converted with a formula. A conversion is read from the tables of a standard, for one group of materials. This page does not have those tables built in. It reads values between the rows of the chart that you type or paste from your own standard. It also changes a Vickers, Brinell or Knoop number into MPa, and gives a rule-of-thumb strength for steel.
Enter your values
Check these values
This is off unless you turn it on. Saved entries stay in this browser only. Untick the box to delete them.
Your values are worked out in this browser. They are not sent to a server.
Your result will show here
Fill in the values, then choose the button below them.
Your result
How it was worked out
How to use this converter
- Choose Convert with your own conversion chart.
- Take the conversion chart for your material from your standard, for example ASTM E140 or ISO 18265. Type its rows, or paste two columns of numbers and choose Read into rows. Try an example fills in made-up numbers so that you can see how the page works.
- Type the hardness values that you want to convert, and choose the direction.
- Choose Convert. The page gives each value, says which two rows it lies between, and draws your chart as a curve. You can print the result or download it as a CSV file.
- To use the chart again, save it on this device or download it as a file that you can open here later.
Why there is no single formula
Each hardness test presses a different body into the material with a different force and measures something different: the size of the mark, its depth, or how far a small hammer bounces back. How these numbers go together depends on how the material hardens as it is pressed. Steel, stainless steel, brass, aluminium and cast iron all behave in their own way.
So the standards give separate tables for separate groups of materials, made from many tests. A value that you read from a table for steel is wrong for brass. This is also why this page does not offer one chart for everything.
What the page works out
- Between two rows it draws a straight line: value = lower value + (upper value − lower value) × (hardness − lower hardness) ÷ (upper hardness − lower hardness).
- On a row it gives the value of that row.
- Outside the chart it gives no value. A conversion chart must not be stretched past its ends.
- A Vickers, Brinell or Knoop number as a pressure: these numbers are a force in kilograms-force on an area in square millimetres, so 1 unit is 9.80665 MPa. The scale stays the same.
- Rough tensile strength of steel: about 3.45 MPa for each Brinell point. This is a rule of thumb, not a table, and the page says so in the result.
Worked example
A chart. Take the made-up example chart with the rows 20 → 150 and 30 → 225. A hardness of 25 is halfway between the two rows, so the value is 150 + (225 − 150) × 0.5 = 187.5. A hardness of 60 is above the last row of that chart, so the page gives no value.
A pressure. HV 700 × 9.80665 = 6864.655 MPa, which is 6.865 GPa. It is still a Vickers hardness.
Steel strength. A carbon steel of 200 HBW has a tensile strength of about 200 × 3.45 = 690 MPa by the rule of thumb.
Limits you should know
- The page has no conversion tables of its own. It cannot convert a hardness unless you give it the chart for your material.
- It cannot check your chart. A wrong row gives a wrong answer. Look at the curve of your chart: a row that is out of line shows up there.
- A converted hardness is less sure than a measured one. Standards use a conversion only when the wanted test cannot be made, and the report names the scale that was really measured.
- A straight line between two rows is a small approximation. Use the rows of the standard as closely spaced as it gives them.
- The rule of thumb for tensile strength is only for carbon and low-alloy steels from 100 to 450 HBW. It is not for stainless steel, cast iron, aluminium or copper alloys, and it is not for a design or an acceptance decision.