Toolvito

Works on this device

Concrete Shrinkage Calculator

Concrete shrinks as it dries and as the cement reacts. This page estimates the shrinkage strain of a member at an age by the model of Eurocode 2 (EN 1992-1-1), and how much a free member of a given length shortens.

Enter your values

The drying and autogenous shrinkage strain of a member at an age, and at the end, by EN 1992-1-1:2004 clause 3.1.4 and Annex B.

Your values

The cylinder strength of the strength class, for example 30 MPa for C30/37. EN 1992-1-1 covers 12 to 90 MPa.

Eurocode 2 takes about 50% for dry air inside buildings and about 80% for humid air outside. Use the value for your site.

The age at which you want the shrinkage, in days from casting.

Drying shrinkage starts when curing stops.

More options

Gives how much a free member of this length shortens.

Your values are worked out in this browser. They are not sent to a server.

Your result will show here

Fill in the values, then choose Calculate.

How to use this calculator

  1. Choose Shrinkage strain by Eurocode 2.
  2. Type the strength class fck (the box starts empty; Try an example fills in 30 MPa), choose the cement class and type the relative humidity of the air.
  3. Choose the shape of the member and type its size. The tool works out the notional size h0 = 2 Ac ÷ u.
  4. Type the age you want and the age at the end of curing. Under More options you can type a length to get the shortening.
  5. To turn a strain you already have into a length change, choose Length change for a strain.

The model (EN 1992-1-1:2004 3.1.4 and Annex B)

  • Total: εcs = εcd + εca.
  • Drying: εcd(t) = βds(t, ts) × kh × εcd,0, with βds = (t − ts) ÷ ((t − ts) + 0.04 √h0³) and h0 in mm.
  • Basic drying strain: εcd,0 = 0.85 [(220 + 110 αds1) exp(−αds2 fcm ÷ 10)] × 10⁻⁶ × βRH, with βRH = 1.55 [1 − (RH ÷ 100)³], fcm = fck + 8 MPa, and αds1 = 3, 4, 6 and αds2 = 0.13, 0.12, 0.11 for cement class S, N and R.
  • kh (Table 3.3): 1.0 for h0 = 100 mm, 0.85 for 200 mm, 0.75 for 300 mm and 0.70 for 500 mm or more.
  • Autogenous: εca(t) = (1 − exp(−0.2 √t)) × 2.5 (fck − 10) × 10⁻⁶, with t in days.
  • Length change: ΔL = ε × L.

Worked example

A slab 200 mm thick dries from both faces, so h0 = 200 mm and kh = 0.85. It is C30/37 (fck = 30 MPa, fcm = 38 MPa) with class N cement in air of 60% humidity, cured for 7 days.

βRH = 1.55 × (1 − 0.6³) = 1.215 and εcd,0 = 0.85 × 660 × exp(−0.456) × 1.215 × 10⁻⁶ = 432.1 × 10⁻⁶. At one year, βds = 358 ÷ (358 + 113.1) = 0.760, so εcd = 0.760 × 0.85 × 432.1 = 279.1 × 10⁻⁶. The autogenous part is 0.978 × 50 = 48.9 × 10⁻⁶, and the total 328.0 × 10⁻⁶. In the end the model gives 417.3 × 10⁻⁶.

A free slab 30 m long would shorten by 328.0 × 10⁻⁶ × 30 m = 9.8 mm in that year. A known strain of 400 × 10⁻⁶ on 30 m gives 12 mm.

Limits you should know

  • This is one model with its own range: normal-weight concrete of C12/15 to C90/105. Eurocode 2 states that real shrinkage may differ by about 30 percent; tests of the mix give better values. Your National Annex may change parts of the model.
  • It gives the strain of free concrete. A restrained member cracks or is stressed instead; joints and reinforcement are design questions.
  • The ACI 209R model and other models are not built. For the water–cement ratio and strength, see the Concrete Water Cement Ratio Calculator and the Concrete Strength Estimator.
  • The engineer of record and the code in force decide the design. It is not professional advice.

Related tools